Airgead Cóimhiotal prásála | Comhdhéanamh ceimiceach (%) | Solad | Leachtaigh | Sonraíocht (mm) | Caighdeáin |
Bag10Cuzn (HL301) | AG: 9.0-11.0 Cu: 52.0-54.0 Zn: 35.0-39.0 Eile: Max0.15 | 815ºC | 850ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | Fiontar |
Bag15cuzn | AG: 14.0-16.0 Cu: 46.0-48.0 Zn: 36.0-40.0 Eile: Max0.15 | 750ºC | 830ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | Fiontar |
Bag18cuzn | Ag, Cu, Zn | 700ºC | 815ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | Fiontar |
Bag20cuzn | AG: 19.0-21.0 Cu: 43.0-45.0 Zn: 34.0-38.0 Eile: Max0.15 | 690ºC | 810ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | GB/T10046-2008 EN1044: 1999 AG206 |
Bag25cuzn (HL302) | AG: 24.0-26.0 Cu: 39.0-41.0 Zn: 33.0-37.0 Eile: Max0.15 | 700ºC | 790ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | GB/T10046-2008 EN1044: 1999 AG205 ISO 17672: 2010 AG225 |
Bag30Cuzn | AG: 29.0-31.0 Cu: 37.0-39.0 Zn: 30.0-34.0 Eile: Max0.15 | 680ºC | 765ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | GB/T10046-2008 AWS A5.8 Mála-20 EN1044: 1999 AG204 ISO 17672: 2010 AG230 |
Bag35Cuzn | AG: 34.0-36.0 Cu: 31.0-33.0 Zn: 31.0-35.0 Eile: Max0.15 | 685ºC | 775ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | GB/T10046-2008 AWS A5.8 Mála-35 |
Bag44cuzn | AG: 43.0-45.0 Cu: 29.0-31.0 Zn: 24.0-28.0 Eile: Max0.15 | 675ºC | 735ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | GB/T10046-2008 EN1044: 1999 AG203 ISO 17672: 2010 AG244 |
Bag45Cuzn (HL303) | AG: 44.0-46.0 Cu: 29.0-31.0 Zn: 24.0-27.0 Eile: Max0.15 | 665ºC | 745ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | GB/T10046-2008 AWS A5.8 Mála-5 |
Bag50Cuzn (HL304) | AG: 49.0-51.0 Cu: 33.0-35.0 Zn: 14.0-18.0 Eile: Max0.15 | 690ºC | 775ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | GB/T10046-2008 AWS A5.8 Mála-6 |
Bag60Cuzn | AG: 59.0-61.0 Cu: 25.0-27.0 Zn: 12.0-16.0 Eile: Max0.15 | 695ºC | 730ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | GB/T10046-2008 EN1044: 1999 AG202 |
Bag65Cuzn (HL306) | AG: 64.0-66.0 Cu: 19.0-21.0 Zn: 13.0-17.0 Eile: Max0.15 | 670ºC | 720ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | GB/T10046-2008 AWS A5.8 Mála-9 |
Bag70Cuzn (HL307) | AG: 6.0-7.0 Cu: 19.0-21.0 Zn: 8.0-12.0 Eile: Max0.15 | 690ºC | 740ºC | Slat/sreang/fáinne/árasán ≥φ0.2 Stiall/crios/scragall /preforming Tiús ≥0.05 2.0≤Width≤100 | GB/T10046-2008 AWS A5.8 Mála-10 |