0Cr27Al7Mo2 0Cr13Al4 0Cr25Al5 sreang cóimhiotal téimh leictreach fecral
Grád | 0Cr25Al5 |
Méid | 0.1-1.2mm |
Dromchla | geal annealed |
Meáchan | 1-3kg / rolla |
Friotaíocht | 1.42±0.07μΩ.m |
Teocht is airde | 1250 ℃ |
Dlús | 7.1g/cm³ |
Neart teanntachta | 750N/mm² |
Fadú | ≥12% |
Grád | Teocht is airde | Friotaíocht | Leáphointe | Neart teanntachta | Fadú |
0Cr21Al4 | 1100 ℃ | 1.23±0.06μΩ.m | 1500 ℃ | 750 | ≥12 |
0Cr25Al5 | 1250 ℃ | 1.42±0.07μΩ.m | 1500 ℃ | 750 | ≥12 |
0Cr23Al5 | 1300 ℃ | 1.35±0.06μΩ.m | 1500 ℃ | 750 | ≥12 |
0Cr21Al6NbCo | 1350 ℃ | 1.43±0.07μΩ.m | 1510 ℃ | 750 | ≥12 |
0Cr27Al7Mo2 | 1400 ℃ | 1.53±0.07μΩ.m | 1520 ℃ | 750 | ≥10 |
KSC | 1350 ℃ | 1.44±0.05μΩ.m | 1510 ℃ | 750 | ≥16 |
Cr20Ni80 | 1200 ℃ | 1.09±0.05μΩ.m | 1400 ℃ | 750 | ≥20 |
Cr15Ni60 | 1150 ℃ | 1.12±0.05μΩ.m | 1390 ℃ | 750 | ≥20 |
Cr20Ni35 | 1100 ℃ | 1.04±0.05μΩ.m | 1390 ℃ | 750 | ≥20 |
Cr20Ni30 | 1100 ℃ | 1.04±0.05μΩ.m | 1390 ℃ | 750 | ≥20 |
Grád | Comhdhéanamh ceimiceach % | ||||||||
C | P | S | Mn | Si | Cr | Ni | Al | Fe | |
≤ | |||||||||
0Cr21Al4 | 0. 12 | 0. 025 | 0. 025 | 0.7 | ≤1.0 | 17-21 | ≤0.6 | 3-4 | cothromaíocht |
0Cr25Al5 | 0. 06 | 0. 025 | 0. 02 | 0.5 | ≤0.6 | 23-26 | ≤0.6 | 4.5-6.5 | cothromaíocht |
0Cr23Al5 | 0. 06 | 0. 025 | 0. 02 | 0.5 | ≤0.6 | 20.5-23.5 | ≤0.6 | 4.2-5.3 | cothromaíocht |
0Cr21Al6Nb | 0. 05 | 0. 025 | 0. 02 | 0.5 | ≤0.6 | 21-23 | ≤0.6 | 5-7 | cothromaíocht |
0Cr27Al7Mo2 | 0. 05 | 0. 025 | 0. 02 | 0.2 | ≤0.4 | 26.5-27.8 | ≤0.6 | 6-7 | cothromaíocht |
Cr20Ni80 | 0. 08 | 0. 02 | 0. 015 | 0.6 | 0.75-1.6 | 20-23 | cothromaíocht | <0.5 | ≤1.0 |
Cr15Ni60 | 0. 08 | 0. 02 | 0. 015 | 0.6 | 0.75-1.6 | 15-18 | 55-61 | <0.5 | cothromaíocht |
Cr20Ni35 | 0. 08 | 0. 02 | 0. 015 | 1.0 | 1-3 | 18-21 | 34-37 | - | cothromaíocht |
Cr20Ni30 | 0. 08 | 0. 02 | 0. 015 | 1.0 | 1-3 | 18-21 | 30-34 | - | cothromaíocht |